Thanks Jay, Much Appreciated! Erlihemi, yes, the outgassing was a pain. I feel lucky I have a powder coater nearby who really cares about his work. His process sounded similar if I remember correctly it was just with that piece of metal it was a pain. He also noted when he did the initial warming for outgassing he found that adhesive/glue or something like that flowed out a bit from behind where the horizontal rib meets with all the verticals so he needed to clean all that out. Take Care